Silicon Molybdenum Brick
+
  • Silicon Molybdenum Brick

Silicon Molybdenum Brick


Product Introduction

Silicon molybdenum bricks are made from high-grade bauxite clinker and silicon carbide as the main raw materials, formed under high pressure and fired at high temperatures. The products have high compressive strength at room temperature and high structural strength at elevated temperatures, good thermal shock stability, and continuously form a protective layer during use. They have good wear resistance and strong spalling resistance, making them suitable for areas such as the transition zone, cooling zone, and kiln mouth of cement kilns.

Product Details


  Product Overview:

  Silicon molybdenum bricks are made from high-grade high-alumina bauxite clinker and silicon carbide as the main raw materials, formed under high pressure and fired at high temperatures. The product has high compressive strength at room temperature and high structural strength at high temperatures, good thermal shock stability, and continuously forms a protective layer during use, with good wear resistance and strong spalling resistance, suitable for the transition zone, cooling zone, and kiln mouth of cement kilns.

  Product Details:

  It has good wear resistance, corrosion resistance, spalling resistance, high refractoriness and load softening temperature, as well as excellent thermal shock stability and compressive strength at room temperature; it is not suitable for hanging kiln skin at high temperatures; the insulation layer has a low thermal conductivity, which can achieve the dual function of reducing body temperature and saving energy, significantly extending the life of rotary kilns, making it an ideal lining material for the cooling zone and transition zone of new dry-process cement kilns.

  Physical and Chemical Indicators:

Item ZJAS-1680 ZJAS-1650 ZJAS-1550
 Chemical Composition (%) Al2O3 ≥65 ≥63 ≥60
SiC+SiO2 ≥30 ≥30 ≥30
Bulk Density (g/cm³) ≥2.65 ≥2.60 ≥2.50
Apparent Porosity Rate (%) ≤16 ≤17 ≤18
Compressive Strength at Room Temperature (MPa) ≥90 ≥90 ≥80
Load Softening Temperature, ℃

(0.2MPa, t0.6)
≥1680 ≥1650 ≥1550
 Thermal Shock Stability, times

(1100℃, water cooling)
≥15 ≥15 ≥15
Wear Coefficient (A/C) ≤6 ≤7 ≤8