Magnesium-aluminum spinel brick
+
  • Magnesium-aluminum spinel brick

Magnesium-aluminum spinel brick


Product Introduction

Magnesium-aluminum spinel bricks are products made from high-purity magnesia and pre-synthesized magnesium-aluminum spinel as the main raw materials, through reasonable grading, high-pressure forming, and high-temperature firing.

Product Details


  Product Overview:

  Magnesium-aluminum spinel bricks are products made from high-purity magnesia and pre-synthesized magnesium-aluminum spinel as the main raw materials, through reasonable grading, high-pressure forming, and high-temperature firing. Their characteristics include high self-refractoriness, high strength, resistance to erosion, low linear expansion coefficient, and good thermal shock resistance, making them ideal refractory materials for the transition zone of cement rotary kilns.

  Product Details:

  Alumina-based sintered magnesium-aluminum spinel uses high-quality bauxite with an Al203 content of over 76% and high-quality light-burned magnesia powder with an MgO content of over 95%. After a multi-stage homogenization process, it is sintered at high temperatures above 1800°C in an ultra-high temperature tunnel kiln, resulting in high bulk density, high mineral phase content, well-developed grains, uniform structure, and stable quality. Magnesium-aluminum spinel has good erosion resistance, strong corrosion and spalling resistance, good slag resistance, wear resistance, good thermal shock stability, and high-temperature resistance. It is an ideal raw material for producing magnesium-aluminum spinel bricks for the high-temperature zone of cement rotary kilns, steel ladle lining bricks, and steel ladle castables. Magnesium-aluminum spinel is widely used in refractory materials, steelmaking, cement rotary kilns, and glass industrial kilns.

  Physical and Chemical Indicators:

Item ZJMA-6 ZJMA-7 ZJMA-8
Chemical Composition (%) MgO ≥85 ≥86 ≥86
Fe₂O₃ ≤0.7 ≤0.7 ≤0.7
Al₂O₃ 11-13 10-12 10-12
SiO₂ ≤0.7 ≤0.5 ≤0.35
CaO ≤1.3 ≤1.1 ≤0.95
Bulk Density (g/cm³) ≥2.95 ≥2.97 ≥3.0
Apparent Porosity (%) ≤16 ≤16 ≤16
Room Temperature Compressive Strength (MPa) ≥65 ≥65 ≥65
Softening Temperature under Load, °C
(0.2MPa, t0.6)
≥1700 ≥1700 ≥1700
Thermal Shock Stability, times
(1100°C, water cooling)
≥10 ≥12 ≥12

Keywords:

Kiln Display


Nodata

Feedback

Leave an online message and get free product quotes